Galvanic Corrosion in PV Mounting Fasteners: Stainless Against Galvanised Steel

  • Home
  • Science and technology
Galvanic Corrosion in PV Mounting Fasteners: Stainless Against Galvanised Steel

Galvanic Corrosion in PV Mounting Fasteners: Stainless Against Galvanised Steel

The most common pairing on PV structures is galvanised steel sections with stainless fasteners: the first is cheap and strong, the second resists corrosion with stable strength. In dry regions the combination serves for years. In wet and chloride-bearing environments trouble starts around the bolt holes - white rust on the zinc, then thinning of the hole wall, then a loose connection. This is not a screw defect but galvanic corrosion between two metals in contact, and we meet it on project after project.

Three conditions for galvanic corrosion

Galvanic corrosion needs three things at once: two metals at different potentials, an electrolyte connecting them, and electrical contact between them. On a PV structure all three occur naturally - stainless and galvanised steel differ clearly in potential, rain, condensation and humid air supply the electrolyte, and the bolt clamps the two into good contact. Given all three, corrosion proceeds and only the rate is in question. The strategy is therefore to break at least one condition, not to eliminate corrosion.

How the stainless-galvanised couple behaves

In this couple stainless is the nobler metal and becomes the cathode; it barely corrodes and actually alkalinises its surroundings through the cathodic reaction. The zinc and steel substrate are the anode and dissolve faster. Failure therefore always appears on the bracket side, not on the screw, which is why customers misdiagnose it: the removed screw looks new while the bracket hole is rusted through. Understanding the direction puts protection where it belongs, on the connected part.

Why the area ratio sets the rate

Anodic dissolution scales with cathode area and inversely with anode area. A bolt as a small cathode against a large bracket anode is actually the favourable direction, since the anode current density is spread thin. The dangerous case is the reverse: galvanised parts on a stainless structure, or a locally breached coating that leaves a small anode facing a large stainless cathode, where anode current density is extreme and the breach perforates quickly. Design for large anodes and avoid small ones.

Environment: humidity, chloride, temperature

An electrolyte is the precondition, so humidity dominates. Below a certain relative humidity a continuous water film cannot form and the couple current is small; above it, corrosion runs continuously. Chloride raises conductivity and attacks the passive film, multiplying the rate, which is why coastal and industrial sites suffer most. Higher temperature speeds the reaction but also dries surfaces, so the net effect depends on wet time - and intermittent wetting is often harsher than permanent immersion.

Practical isolation

Electrical isolation is the direct answer: insulating washers under head and nut, and a sleeve through the hole, break the galvanic path. Simple in principle, with caveats. The insulator must be weather resistant, since ordinary nylon ages and cracks under UV and heat. It needs enough thickness and hardness not to be crushed. It must not be scratched during assembly. Its aging life must match the plant design life. Skip any of these and isolation only postpones failure.

The limits of coating and galvanising

Coating or thicker zinc works by moving the anode from steel to zinc, spending zinc to protect steel. Effective, with boundaries: a breach becomes a small anode and corrosion concentrates there; uneven thickness fails first at the thinnest point; cut edges and hole walls are usually thinnest. Recoat holes and cuts made on site, inspect for scratches after installation and touch them up. Treating coating as an absolute barrier while ignoring damage is why so many sites rust in years five to eight.

Recognising the failure

Start with location: concentration near dissimilar-metal contact faces, along crevices, fading outward from contact points fits galvanic attack. Then read the products - white or grey powder for zinc, red-brown for steel, deep pits with little red rust for stainless pitting. Where needed, section the part and look for selective dissolution and pit morphology. Put that together with the site environment record to separate galvanic corrosion from simple coating defects and mechanical damage.

A design-stage checklist

A workable checklist: unify materials where possible and reduce dissimilar contact; where that is impossible, rank by potential difference and isolate the worst pairs; avoid small-anode geometry; recoat after drilling; specify insulator material and aging requirements; mark contact-face treatment on the drawing; and state the corrosivity category and verification method in the technical agreement. We review bracket and fastener material pairing with customers early and supply insulated washer kits where needed.

Contact