Galvanic Corrosion Between PV Clamp Bolts and Aluminium Substrates

  • Home
  • Science and technology
Galvanic Corrosion Between PV Clamp Bolts and Aluminium Substrates

Galvanic Corrosion Between PV Clamp Bolts and Aluminium Substrates

PV module frames are mostly aluminium alloy while clamps are usually stainless or hot dip galvanized steel. Each material resists corrosion on its own, yet together they cause trouble: the potential difference between stainless and aluminium approaches half a volt, and once an electrolyte bridges them the aluminium becomes the sacrificial side. The white powder, frame pitting and corroded clamp roots seen at real plants largely trace to this mechanism. Zhuhai Jiali Hardware has handled such field feedback on PV fasteners, and this article explains the cause and prevention.

Three Conditions Must Coexist

The first is a large enough potential difference. The greater the difference, the higher the driving voltage. Stainless with aluminium is a wide gap, carbon steel with aluminium is also risky, while aluminium with aluminium and stainless with stainless essentially avoid the problem.

The second is electrical contact, usually achieved by direct metal-to-metal contact. The third is an electrolyte, and rain, condensation and washing water all provide ion paths, while a PV plant is outdoors by definition. In practice all three conditions coexist almost always.

The question is therefore not whether corrosion occurs but how fast. Rate depends on area ratio, humidity, chloride concentration and temperature, and those are designable variables.

Area Ratio: It Sets Severity and Is Rarely Discussed

Galvanic severity depends strongly on the ratio of cathode area to anode area. A larger cathode raises current density on the anode and concentrates attack. The surface area of a clamp bolt is usually far smaller than that of the aluminium frame, so when aluminium is the anode the corrosion concentrates in the small contact region, producing visible pits around the bolt.

Conversely, if aluminium must contact stainless, the anode area should be as large and the cathode area as small as possible. This rule directly affects outcomes when sizing clamps and shaping contact faces.

What Shows Up on Site

The most common symptom is white powder, the corrosion product of aluminium, typically appearing around contact faces and especially after rain. The powder itself is not structural, but it proves corrosion is underway and will gradually thin the contact area.

The second is local pitting in the frame, at the points where aluminium corrodes, from a few tenths of a millimetre to one or two millimetres deep, enough in severe cases to weaken local frame strength. The third is corrosion at the clamp root, which is actually more common with a stainless clamp and stainless bolt, because the crevice holds water and dries slowly.

Approach One: Break the Contact with a Barrier

The most direct method is an insulating layer between the two metals, commonly a nylon washer, an engineering plastic sleeve or a coated washer. Such solutions are inexpensive and effective, with two cautions: the washer must cover the entire contact face rather than part of it, and it must be weather resistant, since ordinary nylon ages and cracks under long UV and humid exposure.

Coatings are another barrier. Anodising an aluminium frame creates an insulating oxide film, and passivation strengthens the passive film on stainless. Both can be scratched during installation, however, and a scratch becomes a new corrosion site.

Approach Two: Change the Material Combination

Switching the clamp to aluminium alloy is the most thorough answer, since identical materials do not corrode galvanically. The cost is lower strength and wear resistance, and threads need a wire insert or a metal-cored structure for reinforcement.

Another direction is a galvanized steel clamp. Zinc is closer to aluminium in potential than stainless is, and as the anode it sacrifices itself to protect the contact zone. With adequate coating thickness this performs reasonably outdoors; the risk is that once the coating is breached the steel substrate corrodes quickly.

Approach Three: Control Environment and Detail Design

Structurally, avoid trapped water. Give the contact face a drainage slope, or cut drainage notches in the clamp base so water does not stand in the crevice. The change is small, the effect on corrosion rate is not.

Environment control is limited but cleaning deserves attention. If module washing uses a chloride bearing agent, chloride remains in the contact zone and accelerates pitting. The cleaning procedure should either exclude high chloride agents or include thorough rinsing afterwards.

How to Verify the Protection Works

Verification works at two levels. In the laboratory, a cyclic corrosion test simulating alternating humidity, salt spray and drying is closer to PV service than plain neutral salt spray, and the focus is corrosion product quantity and pit depth around contact faces.

At site level, periodic inspection does the job. Mark observation points at typical locations, inspect every six or twelve months, and record white powder quantity and pit depth change. Two or three years of such data carries more weight than any laboratory result.

What Procurement Should Confirm

Procurement should settle at least four questions: whether the clamp material and frame material combination has been assessed for galvanic corrosion, whether a barrier washer is included and of what material, what the surface treatment is and how thick, and whether comparable projects have field records. These four questions expose most of the risk early.

Zhuhai Jiali Hardware provides material combination advice and matched insulating parts for PV fasteners and can support cyclic corrosion verification. Over twenty five years of plant life, clamp bolts are a tiny line in the cost structure, but they are among the few parts that cannot be replaced cheaply once they fail.

Contact

Contact: Lizhong Deng

Phone: 13928071304

Tel: +86-756-8586520

Email: sales@jlfastener.com

Add: Room 56-301,Mingzhubeilu 388hao,Xiangzhou Area,Zhuhai City,GuangDong,China