PV racking stays outdoors, facing salt spray, rain, UV and thermal cycling; fastener corrosion and weathering decide long-term reliability. Salt spray evaluates metallic coating resistance, UV aging evaluates coatings and plastics—often combined. This guide covers conditions and judgment.
Environments differ—coastal, inland, desert, plateau—so test plans follow project location and required corrosion grade.
Salt Spray Conditions
Neutral salt spray follows GB/T 10125 or ISO 9227 with controlled concentration, pH, temperature and fallout. PV projects set duration by corrosion grade; hot-dip galvanized and coated parts are judged differently.
Evaluation covers corroded area, coating loss and base rust. Galvanized parts track white and red rust onset; coated parts track blistering, peeling and scribe creep.
UV Aging Conditions
UV aging follows GB/T 16422.3 or ISO 4892-3, using fluorescent UV lamps with condensation or spray to mimic rain and dew in cycles, with irradiance, temperature and humidity per standard.
Metrics include color difference, gloss retention, chalking, cracking and adhesion loss. Coatings and plastics age faster under UV plus moisture—light-only tests miss reality.
Specimens and Cycles
Sample from batches with surfaces matching products, avoiding scratches or contamination. Record coating thickness, system and color before testing.
Cycles follow project requirements and expected life; hours are often converted to outdoor years, but conversion is approximate—results serve comparison and screening, not precise life claims.
Combined and Cyclic Testing
Real exposure combines salt spray, UV, temperature, humidity and mechanical load; combined tests better reflect failure. A common approach alternates salt spray and UV with humidity stages.
For racking joints, add vibration or load cycling to assess corrosion plus stress. Combined conditions are complex—specify each stage in the plan.
Judgment and Acceptance
Judge per project spec or company standard: no red rust affecting strength, no coating peel to base, color and gloss within allowance.
Use standard photos and rating charts to cut subjectivity. Critical parts may add post-corrosion mechanical sampling to confirm margin.
Applying Results
Results guide coating selection, supplier evaluation and acceptance. Compare schemes under identical conditions to avoid misjudgment.
Combine data with site inspection to calibrate life expectations and maintenance. Analyze failures and feed back to thickness, coating and installation improvements.
Comparing Coating Systems
Compare systems on the same substrate, film thickness and conditions; otherwise conclusions fail. Hot-dip zinc, zinc-aluminum and powder coatings fail differently, so metrics differ.
Record thickness, adhesion and edge coverage—edges and holes are weak points. Flat-panel results overstate product performance.
Use comparisons for selection, but combine with environmental class and life-cycle cost.